| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Nilit FRIANYL B63 SG-GV 2515 Nylon 6 for injection molding, 25% mineral filled and 15% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Nilit FRIANYL B63 SG-GV20 Nylon 6 for injection molding, 20% glass fiber reinforced
Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | |
|
Radici Radilon® A RV250 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D638 |
|
Gharda Chemicals Gafone S 1320GF Polysulfone (PS)
(discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC
LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare.
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
|
DSM Akulon® K224-G3U (Dry) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Grupo Repol Dinalon® A1S25 G15 PA66 15% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | Conditioned; ISO 527-1/-2 |
|
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber
PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KFL34XXC Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL34XXC is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East)
VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts.
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 1mm/min; ISO 527 |
|
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-2/5 |
|
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF
Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific)
Modified PPO Resin with 20% Glass Fibre Reinforced
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding...
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
|
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® BM-30 PA6-MD30
Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
|
EMS-Grivory Grivory® LV-3H PA12-GF30
Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 50%RH; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | DAM; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 50%RH; ISO 527-1/-2 |
|
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black
Information provided by Eurotec®
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527-1,-2 |
|
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
|
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**
15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resi..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
|
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
|
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Tensile Modulus | 6.50 GPa | 943 ksi | cond.; ISO 527-1, -2; 1 mm/min |
|
Lanxess Durethan® BKV 35 CX H2.0 900876 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||