Polymer Property : Shear Modulus = 473 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Shear Modulus 3.26 GPa
473 ksi
Calculated
Plenco 2369 Phenolic, Granular, Compression Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..