| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 5118P (18602) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527 |
|
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | >= 30.0 MPa | >= 4350 psi | ASTM D882 |
|
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Braskem HM 150 HDPE Monofilament Polyethylene
(discontinued **)
Applications: Raschel; flat yarn; general and industrial rape netting. Information provided by Braskem
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film
Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film (
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® CR 9 HV PA*
Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® CR 9 PA*
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6
Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® F 40 NL PA6
Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® F 47 NL nat 6028 PA6
Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM-D882 |
|
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene
HDPE GM9450F is a high-density polyethylene developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and e..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
Total XSene® HD55110 High Density Polyethylene - Blown Film
HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | Average value: 30.0 MPa Grade Count:6 |
|
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ASTM D882 |
|
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom..
|
|||
| Film Tensile Strength at Yield, TD | 30.0 MPa | 4350 psi | ISO 527-3 |
|
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..
|
|||