| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 - 359 MPa | 13000 - 52000 psi | Average value: 152 MPa Grade Count:20 |
|
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 - 110 MPa | 13000 - 16000 psi | Average value: 98.7 MPa Grade Count:8 |
|
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
|
|||
| Flexural Yield Strength | 89.8 MPa | 13000 psi | ASTM D790 |
|
Plenco 4100 Phenolic, Granular, Injection Molded
(discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
|
|||
| Flexural Yield Strength | 89.8 MPa | 13000 psi | ASTM D790 |
|
Plenco 6802 Phenolic, Granular, Transfer Molded
(discontinued **)
Two-Stage Phenolic. PLENCO 06802 is a mica and mineral filled novolac phenolic molding compound. Available in Brown.Information supplied by Plenco
|
|||
| Flexural Yield Strength | 89.6 - 372 MPa | 13000 - 54000 psi | Average value: 249 MPa Grade Count:13 |
|
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Electrafil® DB-50/SS/6/FR Polycarbonate, 6% Stainless Steel Fiber (dry blend), Flame Retardant |
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES HiFill FR® PC FR SFX-ORANGE 1.0
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: OrangeInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES HiFill FR® PC FR X
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Flame Retardant and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Spartech Royalite R910 PC/ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, ..
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plaslube® NY-1/TF/10 Nylon 66, 10% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin..
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PC/ABS FR 2810
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
|
|
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend) |
|||