| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength | 160 MPa | 23200 psi | ASTM D790 |
|
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Flexural Yield Strength |
160
MPa <br>@Temperature 90.0 °C
|
23200
psi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | |
|
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | Flexural Strength |
|
MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite
Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated,..
|
|||
| Flexural Yield Strength |
160
MPa <br>@Strain 3.50 %
|
23200
psi <br>@Strain 3.50 %
|
2 mm/min; ISO 178-A |
|
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber
PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1010A PEI
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), ..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics ULTEM HU2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM AUT200 PEI
Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East)
Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | ASTM D790 |
|
Techmer ES HiFill® TPX-HTN-01026 A 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File ..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF003AS PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF003AS is a compound based on Polyphthlamide resin containing Glass Fiber. Added features include; Heat Stabilized.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | ISO 178 |
|
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | ASTM D790 |
|
E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Yield Strength | 160 MPa | 23200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East)