| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength |
195
MPa <br>@Temperature 90.0 °C
|
28300
psi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ASTM D790 |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | |
|
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | |
|
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | |
|
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled
Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ISO 178 |
|
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFP36XXZ PA 66 (Asia Pacific)
LNP Lubricomp RFP36XXZ is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: internally lubricated. Also known as Lubricomp RFL-4536 ..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 420HP PBT
30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ASTM D790 |
|
Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE+ Silicone LubricantFeatures: Lubricated, Heat Stabilizer and Good W..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® HX420HP PBT
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East)
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East)
Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ISO 178 |
|
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ASTM D790 |
|
E-Polymers TEKAMID® TA210SG30 Impact Modified, 30% Glass Fiber Reinforced PA66, DAM
30% Glass Fiber reinforced, Impact resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Yield Strength | 195 MPa | 28300 psi | ASTM Data |
|
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. ..
|
|||