Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 76.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
NYCOA 1637 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® HMG47MD ABS
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
Flexural Yield Strength 76.0 MPa
11000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® MG38U ABS
High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance.
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS
High impact PC+ABS material designed for local Pacific Automotive applications
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific)
High impact PC+ABS material designed for local Pacific Automotive applications
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East)
High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Ineos Nova 2590 General Purpose Crystal Polystyrene  (discontinued **)
Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Ineos Nova 4214 Medium Impact Polystyrene  (discontinued **)
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o..
Flexural Yield Strength 76.0 MPa
11000 psi
at 5% strain; ASTM D790
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam  (discontinued **)
Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound  (discontinued **)
Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat re..
Flexural Yield Strength 76.0 - 109 MPa
11000 - 15800 psi
Average value: 85.6 MPa Grade Count:15
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Ineos Nova 1300 High Heat Crystal Polystyrene
High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation..
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
LG Chemical RS-650 ABS, Extrusion, General Purpose
Information Provided by LG Chem
Flexural Yield Strength 76.0 MPa
11000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific)
PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
Flexural Yield Strength 76.0 MPa

@Strain 3.50 %
11000 psi

@Strain 3.50 %
2 mm/min; ISO 178
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Ineos Nova 2500 General Purpose Crystal Polystyrene  (discontinued **)
Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi..
Flexural Yield Strength 76.0 - 110 MPa
11000 - 16000 psi
Average value: 93.0 MPa Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Flexural Yield Strength 76.0 MPa
11000 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Ineos Nova 1301 High Heat Crystal Polystyrene
High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plenco 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties...
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plaslok 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 304 is a two-stage, woodflour and cel..
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Plaslok 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 501 is a two-stage, mineral and flock..
Copyright © lookpolymers.com All Rights Reserved