| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 - 138 MPa | 13000 - 20000 psi | Average value: 109 MPa Grade Count:6 |
|
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
ASTM D790 |
|
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 - 110 MPa | 13000 - 16000 psi | Average value: 98.7 MPa Grade Count:8 |
|
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
|
|
KEP Kepital® F20 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Star Plastics PC703 Molding Grade PC with release
Information provided by Star Plastics, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Luriblend® POM HO TL2 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK MB Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho..
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho..
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PC/ABS FR 1950 BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PC/ABS FR 2810
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Techmer ES Plastiblend® PC/PET IM 1016 UV
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc.
|
|||
| Flexural Yield Strength |
89.6
MPa @Thickness 3.17 mm |
13000
psi @Thickness 0.125 in |
|
|
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Clariant Renol BR7140 Polycarbonate/ABS Alloy
Data provided by Clariant Masterbatches
|
|||
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
|
Clariant Renol PA2SP0023 Nylon 6, Impact and Flow Modified, ESD Protection
Data provided by Clariant Masterbatches
|
|||