| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycolac® INP572 ABS
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific)
Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer
High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific)
Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East)
Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® ML7691 PC
UV stabilized clear polycarbonate formula for internal uses only.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East)
Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific)
LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||