| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 0.701 kN/m | 4.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP017102 White Polyester Label Products
3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permane..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M PS195 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M PS197 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ 1000-31 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
|
3M Scotchcal™ 1000-77 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic and uncoated, clear polycarbonate |
|
3M Scotchcal™ 3632-156 Translucent Film
2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
|
3M Scotchcal™ 50-64 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panel |
|
3M Scotchcal™ 8000-114 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ 8000LF-13 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ ElectroCut™ 7125-11 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ ElectroCut™ 7125-11 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ ElectroCut™ 7125-13 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
|
3M Scotchcal™ ElectroCut™ 7125-177 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ ElectroCut™ 7125-186 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Fruehauf pre-painted panels |
|
3M Scotchcal™ ElectroCut™ 7125-89 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ ElectroCut™ 7125-99 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
|
3M Scotchcal™ ElectroCut™ 7725-197 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ 1000-131 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
|
3M Scotchcal™ 50-58 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Urethane paints |
|
3M Scotchcal™ ElectroCut™ 7125-139 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
|
3M Scotchcal™ ElectroCut™ 7125-276 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic |
|
3M Scotchcal™ ElectroCut™ 7125-49 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Polycarbonate |
|
3M Scotchcal™ ElectroCut™ 7125-53 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ ElectroCut™ 7725-130 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ ElectroCut™ 7725-20 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ ElectroCut™ 7725-41 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ ElectroCut™ 7725-49 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ ElectroCut™ 7725-85 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ 1000-63 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.701 kN/m | 4.00 pli | Adhesion to ABS |
|
3M Scotchcal™ 1000LF-120 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||