| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 0.877 - 1.75 kN/m | 5.00 - 10.0 pli | T-peel, Al to Al |
|
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System
Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | 72 hour RT glass, 90° peel, 2 mil aluminum foil backing |
|
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | After Thermal Stress; IPC TM-650 2.4.8 |
|
Arlon 25N Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data ..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon R32089R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Steel; ASTM D3330 |
|
3M Scotch® 890MSR Filament Tape
Scotch® Filament Tape 890MSR is a high performance transparent filament tape reinforced along its length with continuous polyester-yarn filaments, which gives the tape a very high tensile strength...
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-41 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-57 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-89 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Alodine, aluminum |
|
3M Scotchcal™ 50-84 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 8000LF-10 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 8626 ES Clear Graphic Film
Film 8626 ES is a 2 mil, clear graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and outdo..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7125-187 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-105 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | T-Peel |
|
3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer
High Temperature strength and High ViscosityInformation provided by 3M
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon 44566R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon 44576XB015 0.015" (0.381 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum and rubber on fiberglass clothThis data represents typical values for the production ma..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Stainless Steel, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M 7053 Screen Printable Vinyl Performance Label Products
3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
|
3M 7620/7890 White Vinyl Label Material
3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick ta..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | 72 hour RT glass, 90° peel, 2 mil aluminum foil backing |
|
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Stainless Steel, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
|
3M 9442 Adhesive Transfer Tapes with Adhesive 350
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Polypropylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
|
3M 9485EK Adhesive Transfer Tapes with Adhesive 350
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength (Rubber to Rubber) |
|
Arlon R31310R012 Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Aluminized PET FilmSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material ..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 8000-17 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7125-31 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-307 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-37 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 - 7.01 kN/m | 5.00 - 40.0 pli | Varies with substrates. |
|
Loctite® Durabond® E-90FL Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
|
|||