| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Aluminum, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
|
3M 9675 Adhesive Transfer Tapes with Adhesive 350
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8000-12 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8626 ES Clear Graphic Film
Film 8626 ES is a 2 mil, clear graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and outdo..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
|
3M Scotchlite™ 5100-10 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
|
3M Scotchlite™ 680-72 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum |
|
3M Scotchlite™ 680-82 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 30580R020 0.020" (0.508 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Bond Strength; Arlon SQA-TMS-011 |
|
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 51571XA015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum on fiberglass clothThis data Represents typical values for the production material. T..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 51581R018 0.018" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
|
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 55578XA030M 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R31031R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1564 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for th..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R33706R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R34688XA030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured/Cured LayersThis data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8628 ES Translucent Graphic Film
Film 8628 ES is a 2 mil, translucent graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||