| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 2.63 - 3.51 kN/m | 15.0 - 20.0 pli | |
|
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black
Information provided by ITW Devcon
|
|||
| Peel Strength | 2.63 - 3.51 kN/m | 15.0 - 20.0 pli | |
|
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White
Information provided by ITW Devcon
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle |
|
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | At 100% cohesive failure using 1 in. x 8 in. stainless steel screen at 180° pull angle |
|
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | T-peel |
|
Master Bond EP51FL Toughened and Flexible Adhesive Compound
Master Bond EP51FL is a two component epoxy system for high performance bonding sealing and coating. It combines superior toughness with user friendly handling properties, along with unusually fast ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Al/Al, 30 min cure at 250°F |
|
Master Bond Supreme 3HT-80 One Component, Toughened, Heat Curing Epoxy
Master Bond Polymer System Supreme 3HT-80 is a one component, heat curing epoxy adhesive/sealant featuring excellent physical and chemical resistance properties and a minimal curing temperature of 1..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | T-peel, Al to Al |
|
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant
Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | T-peel, Al to Al |
|
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests
Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | T-peel, Al to Al |
|
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room ..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | T-peel, Al to Al |
|
Master Bond Supreme 33 High Temperature Resistant, Structural Adhesive
Description: Master Bond Polymer System Supreme 33 is a unique, room temperature curing, toughened epoxy adhesive/sealant, offering high temperature resistance. This innovative system offers high bo..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | |
|
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy
Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | |
|
Dow Corning 730 SOLVENT RESISTANT SEALANT
Fluorosilicone (solvent resistant) RTV sealantInformation provided by Dow Corning
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Bond Strength; ASTM D624 |
|
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Bond Strength; Arlon SQA-TMS-011 |
|
Arlon R30711R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | 180° Canvas to Cold Rolled Steel |
|
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | T-Peel |
|
3M Scotch-Weld™ CA100 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-peel and impact strength and high thermal shock and heat resistance.Information provided by 3M..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | 180° |
|
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | To Copper (1/2 oz.); A, TS; IPC TM-650 2.4.8 |
|
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite
Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Adhesion to Lead |
|
3M EPS-200 Tubing
3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Adhesion to Lead |
|
3M EPS-300 Heat Shrink Tubing
3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Adhesion to Lead |
|
3M EPS-400 Heat Shrink Tubing
3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Stainless Steel, RT 90° Angle Peel, 12 in./minute Jaw Speed (308 mm/min.) 72 hour Dwell; ASTM D3330 |
|
3M 4658F Double Coated Removable Foam Tape with Adhesive 100
3M™ Double Coated Removable Foam Tape 4658F is a clear, double coated acrylic foam tape that removes cleanly from many surfaces. 3M™ Adhesive 100 is a firm acrylic adhesive system that offers high..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Glass-Unsupported Vinyl, 180°, Aging 7 Day @ RT |
|
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Glass-Supported Vinyl, 180°, Aging 1 Day @ RT |
|
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Aluminum-Supported Vinyl, 180°, Aging 1 Day @ RT |
|
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | on canvas |
|
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive
Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Al to Al |
|
Resinlab® EP1026HP Epoxy Adhesive
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan..
|
|||
| Peel Strength | >= 2.63 kN/m | >= 15.0 pli | T-peel |
|
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound
Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat..
|
|||
| Peel Strength | 2.63 kN/m | 15.0 pli | Al to Al |
|
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
|
|||