| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength |
0.525
kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.00
pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Steel; ASTM D1000 |
|
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
|
|||
| Peel Strength | 0.526 - 0.877 kN/m | 3.00 - 5.00 pli | Adhesion to Fruehauf pre-painted panels |
|
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Bond Strength; MIL-I-46852C |
|
Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FM06P Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP013 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP021502 Clear Polypropylene Label Product
3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP083 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FV362 Soft Yellow Vinyl Label Products
3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
|
3M Scotchcal™ 50-97 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7125-187 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-114 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to FRP |
|
3M Scotchlite™ 680-71 Reflective Graphic Film
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to FRP |
|
3M Scotchlite™ IJ680-10 Reflective Graphic Film
6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | After 2 week exposure to 71°C, Vinyl-Altro to Treated plywood, 1 surface Bond |
|
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive
Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor..
|
|||
| Peel Strength | 0.526 - 0.877 kN/m | 3.00 - 5.00 pli | Adhesion to Fruehauf pre-painted panels |
|
3M Controltac™ IJ180-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FA039 Matte Clear Acetate Label Products
3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
|
3M FM291 Indoor UL Recognized Clear Polyester Overlaminate Label Products
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FM459 Indoor UL Recognized Clear Polyester Overlaminate Label Products
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP010609 Matte White Polypropylene Label Product
3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
|
3M FS442 Matte Clear Polystyrene Label Products
3M™ Matte Clear Polystyrene Label Products FS442 is a hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, whic..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FV230 Soft Yellow Vinyl Label Products
3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
|
3M Scotchcal™ 50-82 Graphic Film
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a ..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-130 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-177 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-276 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-29 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
|
3M Scotchcal™ ElectroCut™ 7725-307 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FM023 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FV0146N Soft Clear Vinyl Label Products
3M™ Soft Clear Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
|
|||
| Peel Strength |
0.525
kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.00
pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Steel; ASTM D1000 |
|
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
|
|||