| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 0.877 kN/m | 5.00 pli | Copper; IPC-TM-650 2.4.8 |
|
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material
XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | Bond Strength |
|
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Polypropylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
|
3M 9675 Adhesive Transfer Tapes with Adhesive 350
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Aluminum, etched |
|
3M Controltac™ 3690C Graphic Film with Comply™ Adhesive
This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy b..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
|
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Bond Strength (S2 to S2); ASTM D624 |
|
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
|
3M FP022202 White Polypropylene Label Products
3M™ White Polypropylene Label Products FP022202 is a white opaque material that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FP024802 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are clear materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tac..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Steel; ASTM D3330 |
|
3M Scotch® 890MSR Filament Tape
Scotch® Filament Tape 890MSR is a high performance transparent filament tape reinforced along its length with continuous polyester-yarn filaments, which gives the tape a very high tensile strength...
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-17 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-98 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Acrylic enamel |
|
3M Scotchcal™ 3650-114 Graphic Film
2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to ABS |
|
3M Scotchcal™ 3690 Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 3690LF Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 8000-13 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 8000LF-37 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7125-176 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7125-196 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7125-99 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-19 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-63 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-64 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ IJ3650-114 Graphic Film
2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | T-Peel, Steel Solvent Wipe; ASTM D1876-61T |
|
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M
|
|||
| Peel Strength |
0.877
-
1.75
kN/m @Temperature -55.0 °C |
5.00
-
10.0
pli @Temperature -67.0 °F |
Aluminum, T-Peel |
|
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
|
3M FM041902 White Polyester Label Products
3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which ..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-24 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ ElectroCut™ 7725-38 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Peel Strength | 0.877 kN/m | 5.00 pli | Adhesion to Chrome |
|
3M Scotchcal™ 1000-53 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Peel Strength | >= 0.877 kN/m | >= 5.00 pli | [ppi], Bond Strength |
|
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate