| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 518581R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 28601M015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Tan gum on glass fiber fabricThis data represents typical values for the production material. The data ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 41580R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 3690 Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8000-10 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8000-13 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8000-13 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8000LF-10 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8000LF-37 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8626 ES Clear Graphic Film
Film 8626 ES is a 2 mil, clear graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and outdo..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 30580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 30580R020 0.020" (0.508 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon 51586B015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum and rubber on fiberglass clothThis data Represents typical values for the production m..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
|
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Aluminum, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
|
3M 9445 Adhesive Transfer Tapes with Adhesive 350
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt..
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | Bond Strength |
|
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide
Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Bond Strength(S1 to S2); SQA-TMS-011 |
|
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8000-37 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8000-37 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8628 ES Translucent Graphic Film
Film 8628 ES is a 2 mil, translucent graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, etched |
|
3M Scotchcal™ 8628 ES Translucent Graphic Film
Film 8628 ES is a 2 mil, translucent graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | Adhesion to Aluminum, anodized |
|
3M Scotchcal™ 8000-25 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Peel Strength | 1.05 kN/m | 6.00 pli | on canvas |
|
3M Scotch-Weld™ 3750 Tan Hot Melt Adhesive
Low viscosity for high flow rate, increased production and Good hot tack, quick grab for packaging and woodworkingInformation provided by 3M
|
|||
| Peel Strength | >= 1.05 kN/m | >= 6.00 pli | [ppi], Bond Strength |
|
Arlon 48571R006 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
|
|||