| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 0.450 GPa @Temperature 60.0 °C |
65.3 ksi @Temperature 140 °F |
|
| LATI Latamid 6 E02 PA 6, Impact modified Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A... |
|||
| Tensile Modulus | 0.450 GPa @Temperature 120 °C |
65.3 ksi @Temperature 248 °F |
|
| LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
| Tensile Modulus | 0.450 GPa @Temperature 90.0 °C |
65.3 ksi @Temperature 194 °F |
|
| LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
| Tensile Modulus | 0.450 GPa @Temperature 150 °C |
65.3 ksi @Temperature 302 °F |
|
| LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||