| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus |
4.60
GPa @Temperature 23.0 °C |
667
ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
|
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**)
Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 90.0 °C |
667
ksi @Temperature 194 °F |
|
|
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 120 °C |
667
ksi @Temperature 248 °F |
|
|
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 23.0 °C |
667
ksi @Temperature 73.4 °F |
|
|
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 23.0 °C |
667
ksi @Temperature 73.4 °F |
|
|
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 150 °C |
667
ksi @Temperature 302 °F |
|
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
|
|||
| Tensile Modulus |
4.60
GPa @Temperature 90.0 °C |
667
ksi @Temperature 194 °F |
|
|
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
|
|||