| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX2415 PC
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ..
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer
Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1U |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180-1U |
|
Lanxess Durethan® BKV 15 H.3 DUS008 000000 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180-1U |
|
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180-1U |
|
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber
PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1U |
|
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East)
LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate
SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly..
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
80x10x4; ISO 180/1U |
|
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded
Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1U |
|
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
|
|||
| Izod Impact, Unnotched (ISO) |
45.0
kJ/m² <br>@Temperature 23.0 °C
|
21.4
ft-lb/in² <br>@Temperature 73.4 °F
|
conditioned; ISO 180-1U |
|
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||