| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180-1U |
|
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
Conditioned; ISO 180-1U |
|
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180-1U |
|
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180-1U |
|
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modifiedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
d.a.m.; ISO 180-1U |
|
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1U |
|
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
80x10x4; ISO 180/1U |
|
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1U |
|
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1U |
|
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature 23.0 °C
|
30.9
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East)
High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Unnotched (ISO) |
65.0
kJ/m² <br>@Temperature -30.0 °C
|
30.9
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1U |
|
SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East)
High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||