Polymer Property : Tensile Strength = 379 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength 379 MPa

@Diameter 25.4 mm
55000 psi

@Diameter 1.00 in
Rod H02
Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing ..