| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength |
414
MPa @Diameter 12.7 - 25.4 mm |
60000
psi @Diameter 0.500 - 1.00 in |
Rod H02 |
|
Mueller Ecostreamâ„¢ C36300 Copper Zinc Lead Alloy
As one of the low lead alloys offered in the EcoStream™ family of products, Mueller Brass Company’s C36300 alloy provides a viable alternative to those manufacturers who are manufacturing ..
|
|||
| Tensile Strength |
>=
414
MPa @Thickness 76.2 - 101.6 mm |
>=
60000
psi @Thickness 3.00 - 4.000 in |
Tempers T851/T852) |
|
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
|
|||