| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 123 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific)
LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an..
|
|||
| Dart Drop, Total Energy |
169
J @Temperature 23.0 °C |
125
ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
|
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 141R PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 153 PC
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific)
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 201 PC
7.0 MFR, for thicker sections without sinks. Improved flame retardance.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific)
10.5 MFR. Improved flame retardance.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific)
10.5 MFR. Improved flame retardance. Super mold release.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific)
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 943 PC
Opaque colors, medium viscosity, superior flame retardance. UV-stabilized.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 943A PC
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 950 PC
Opaque colors, high viscosity, superior flame retardance.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HF1140R PC
High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HP2R PC
Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HPS2R PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® LI1813R PC
Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | SABIC Method |
|
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific)
Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | SABIC Method |
|
SABIC Innovative Plastics Lexan® LS3 PC (Asia Pacific)
Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® OQ4320R PC
Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific)
Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 141 PC
General purpose polycarbonate with melt flow rate of 10.5.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific)
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific)
Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized.
|
|||
| Dart Drop, Total Energy |
169
J @Temperature 23.0 °C |
125
ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
|
SABIC Innovative Plastics Lexan® FXE143R PC
UV stabilized PC resin for "Illuminate"/Edge Glow Visual Effect. Medium viscosity (10.5 MFR). Nonhalogenated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific)
Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release.
|
|||
| Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
|
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m..
|
|||