| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy |
29.0
J <br>@Temperature 23.0 °C
|
21.4
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific)
BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance ..
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature -40.0 °C
|
21.4
ft-lb <br>@Temperature -40.0 °F
|
F50; ASTM D-3029 |
|
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici..
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature 23.0 °C
|
21.4
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare.
|
|||
| Dart Drop, Total Energy | 29.0 J | 21.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66
LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Dart Drop, Total Energy | 29.0 J | 21.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific)
LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature 23.0 °C
|
21.4
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS
LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic.
|
|||
| Dart Drop, Total Energy | 29.0 J | 21.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
|
|||
| Dart Drop, Total Energy | 29.0 J | 21.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature 23.0 °C
|
21.4
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP STAT-LOY M3000C PP
LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat.
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature 23.0 °C
|
21.4
ft-lb <br>@Temperature 73.4 °F
|
ASTM D3763 |
|
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
|
|||
| Dart Drop, Total Energy |
29.0
J <br>@Temperature -30.0 °C
|
21.4
ft-lb <br>@Temperature -22.0 °F
|
7.22 ft/sec; ASTM D3763 |
|
ExxonMobil Exxtral™ BMV 102W Performance Polyolefin
Product Description: Polyolefin injection molding compound with high flow, good low-temperature impact resistance, and excellent processability for painted, partial painted, and molded-in-color auto..
|
|||
| Dart Drop, Total Energy |
29.0
-
37.0
J <br>@Temperature -40.0 - -40.0 °C
|
21.4
-
27.3
ft-lb <br>@Temperature -40.0 - -40.0 °F
|
Average value: 33.0 J Grade Count:2 |
|
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m..
|
|||