Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 3.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 3412HF PC
20% glass reinforced, high flow PC. UL rated V-1 at 0.059"",
Dart Drop, Total Energy 3.00 - 29.0 J
2.21 - 21.4 ft-lb
Average value: 7.04 J Grade Count:27
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Dart Drop, Total Energy 3.00 - 7.00 J
<br>@Temperature -30.0 - -20.0 °C
2.21 - 5.16 ft-lb
<br>@Temperature -22.0 - -4.00 °F
Average value: 3.75 J Grade Count:3
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK
LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK
LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP
LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE...
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear
LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched
LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East)
LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66
LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT
LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS
LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS (Asia Pacific)
LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX00887C PC
LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI
LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET
LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications.
Dart Drop, Total Energy 3.00 J
<br>@Temperature -30.0 °C
2.21 ft-lb
<br>@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT
LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Dart Drop, Total Energy 3.00 J
<br>@Temperature 23.0 °C
2.21 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Dart Drop, Total Energy 3.00 J
<br>@Temperature -30.0 °C
2.21 ft-lb
<br>@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics NORYL FN215X PPE+PS
Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction.
Copyright © lookpolymers.com All Rights Reserved