Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 5.90 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific)
Extem XH2315 Resin
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East)
LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man..
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12
LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12
LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66
LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66
LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66
LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM 2200F PEI
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific)
LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU2110 PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 508R PBT+PC
30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66
LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific)
LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS
LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC
LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer
LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific)
LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66
LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA
LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP
LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI
LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable.
Dart Drop, Total Energy 8.00 J
<br>@Temperature 23.0 °C
5.90 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6
LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity.
Copyright © lookpolymers.com All Rights Reserved