Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 65.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS
PC/ABS with high stiffness and impact performance
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific)
Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East)
Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER
Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and ..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HPS6 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific)
Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East)
IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® IR2210 PC (Europe-Africa-Middle East)
IR2210 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® IR2240 PC (Europe-Africa-Middle East)
IR 2240 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East)
VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and ..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HP6NR PC
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Asia Pacific)
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It..
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics PC0703R PC (Europe-Africa-Middle East)
PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.
Dart Drop, Total Energy 65.0 J
47.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen..
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC
Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin.
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Dart Drop, Total Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..