| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® 123X PC Copolymer
Improved flow PC with excellent processability and mold release.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® BY2710X PC (Asia Pacific)
BY2710X is a modified Polycarbonate (PC) resin. It is a non-filled, injection moldable grade with UL-94 V0 rating and is available in various opaque color options.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® EX1332T PC
Lexan* EX1332T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and is UV stabilized. It is availab..
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® EX7631T PC
EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East)
Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold..
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific)
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1200-22 Polycarbonate Resin
Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1300-22 Polycarbonate Resin
Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1201-22 Polycarbonate Resin
Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin
Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Dart Drop, Total Energy | 72.0 J | 53.1 ft-lb | 8000 ipm; ASTM D3763 |
|
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
|
Styron CALIBREâ„¢ 301 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Dart Drop, Total Energy |
72.0
J @Thickness 3.20 mm |
53.1
ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
|
Styron CALIBREâ„¢ 303 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Dart Drop, Total Energy |
72.0
J @Temperature 23.0 °C |
53.1
ft-lb @Temperature 73.4 °F |
ASTM D3763 |
|
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
|
|||