| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 34.5 - 74.0 MPa | 5000 - 10700 psi | Average value: 54.2 MPa Grade Count:7 |
|
Overview of materials for Polyphenylene Ether, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values..
|
|||
| Tensile Strength, Ultimate | 60.0 - 74.0 MPa | 8700 - 10700 psi | Average value: 68.0 MPa Grade Count:24 |
|
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Tensile Strength, Ultimate | 37.0 - 74.0 MPa | 5370 - 10700 psi | Average value: 58.8 MPa Grade Count:4 |
|
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Tensile Strength, Ultimate | 34.0 - 74.0 MPa | 4930 - 10700 psi | Average value: 54.7 MPa Grade Count:3 |
|
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
|
|||