Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 110 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.5 - 110 MPa
1810 - 16000 psi
Average value: 75.0 MPa Grade Count:65
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 44.8 - 110 MPa
6500 - 16000 psi
Average value: 74.2 MPa Grade Count:32
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Tensile Strength, Ultimate 38.0 - 110 MPa
5510 - 16000 psi
Average value: 54.5 MPa Grade Count:12
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 16.0 - 110 MPa
2320 - 16000 psi
Average value: 67.9 MPa Grade Count:16
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Tensile Strength, Ultimate 35.0 - 110 MPa
5080 - 16000 psi
Average value: 55.1 MPa Grade Count:85
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 30.0 - 110 MPa
4350 - 16000 psi
Average value: 49.7 MPa Grade Count:131
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Tensile Strength, Ultimate 110 - 110 MPa

@Temperature >=130 °C
16000 - 16000 psi

@Temperature >=266 °F
Average value: 128 MPa Grade Count:1
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Tensile Strength, Ultimate 110 - 110 MPa

@Time 1.80e+7 - 7.20e+7 sec
16000 - 16000 psi

@Time 5000 - 20000 hour
Average value: 128 MPa Grade Count:1
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Tensile Strength, Ultimate 49.6 - 110 MPa
7200 - 16000 psi
Average value: 71.1 MPa Grade Count:12
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Tensile Strength, Ultimate 68.9 - 110 MPa
10000 - 16000 psi
Average value: 81.7 MPa Grade Count:12
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
Tensile Strength, Ultimate 15.0 - 110 MPa

@Temperature 60.0 - 150 °C
2180 - 16000 psi

@Temperature 140 - 302 °F
Average value: 58.4 MPa Grade Count:4
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Tensile Strength, Ultimate 38.0 - 110 MPa
5510 - 16000 psi
Average value: 88.2 MPa Grade Count:25
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 55.0 - 110 MPa

@Temperature 60.0 - 150 °C
7980 - 16000 psi

@Temperature 140 - 302 °F
Average value: 83.8 MPa Grade Count:1
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Tensile Strength, Ultimate 90.0 - 110 MPa
13100 - 16000 psi
ASTM D638
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 90.0 - 110 MPa
13100 - 16000 psi
ASTM D638
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 90.0 - 110 MPa

@Temperature 120 - 160 °C
13100 - 16000 psi

@Temperature 248 - 320 °F
Average value: 100 MPa Grade Count:1
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Tensile Strength, Ultimate 90.0 - 110 MPa
13100 - 16000 psi
Average value: 103 MPa Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Tensile Strength, Ultimate 40.0 - 110 MPa
5800 - 16000 psi
Average value: 84.1 MPa Grade Count:38
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 80.0 - 110 MPa

@Temperature 60.0 - 150 °C
11600 - 16000 psi

@Temperature 140 - 302 °F
Average value: 95.0 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 75.0 - 110 MPa
10900 - 16000 psi
Average value: 88.0 MPa Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Tensile Strength, Ultimate 40.0 - 110 MPa

@Temperature -40.0 - 70.0 °C
5800 - 16000 psi

@Temperature -40.0 - 158 °F
Average value: 75.0 MPa Grade Count:3
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Tensile Strength, Ultimate 20.0 - 110 MPa
2900 - 16000 psi
Average value: 67.7 MPa Grade Count:184
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 45.0 - 110 MPa

@Temperature 60.0 - 150 °C
6530 - 16000 psi

@Temperature 140 - 302 °F
Average value: 73.8 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved