| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | Same value from ASTM and ISO tests; 5 mm/min. |
|
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Tensile Strength, Ultimate | 125 - 143 MPa | 18200 - 20700 psi | Average value: 133 MPa Grade Count:3 |
|
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..
|
|||
| Tensile Strength, Ultimate | 125 - 230 MPa | 18100 - 33400 psi | Average value: 182 MPa Grade Count:27 |
|
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | |
|
Hybrid Plastics Nanoreinforced® PM 1215 Polyimide
The homogeneous dispersion of POSS® cages within polyimide provides enhanced control over chain dynamics which increases the toughness and damage tolerance over conventional polyimide. The chemic..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ISO 527 |
|
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ISO 527 |
|
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | |
|
Wieland 1964 Wilaform Gold
Fine gold. Universally applicable for sheet metals, volumes, pipes, profiles and contacts.Applications: chains, coin/shape, pipesDental
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | cond; ISO 527-1/-2 |
|
DSM Akulon® S223-PG8 PA66-GF40
40% Glass Reinforced, Impact Modified
|
|||
| Tensile Strength, Ultimate |
125
MPa <br>@Temperature 120 °C
|
18100
psi <br>@Temperature 248 °F
|
ISO 527-1/-2 |
|
DSM Stanyl® 46HF4530 PA46-GF30
30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | cond; ISO 527-1/-2 |
|
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized
|
|||
| Tensile Strength, Ultimate |
125
MPa <br>@Temperature 120 °C
|
18100
psi <br>@Temperature 248 °F
|
ISO 527-1/-2 |
|
DSM Stanyl® TW200B6 PA46-CF30
30% Carbon Reinforced, Heat Stabilized, Lubricated
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | dry; ISO 527-1/-2 |
|
DSM Akulon® K224-G3-FC NA99001 PA6-GF15
15% Glass Reinforced
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Petra® 130 FR BK-112 30% Glass Filled PET
Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) |
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ASTM D638 |
|
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ASTM D638 |
|
A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ASTM D638 |
|
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | 5mm/min; ISO 527 |
|
BASF Ultradur S 4090 G6 LS High Speed BK15077 30% Glass Filled PBT
Ultradur S 4090 G6 LS High Speed BK15077 is a high flow, fast cycling with low warpage, 30% glass filled injection molding PBT.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ATSM D638 |
|
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced
A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ASTM D638 |
|
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ASTM data at 5 mm/min. |
|
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | Same value from ASTM and ISO tests; 5 mm/min. |
|
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
|
|||
| Tensile Strength, Ultimate | 125 MPa | 18100 psi | ISO 527 |
|
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
|
|||