Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 170 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa
24700 psi
Same value from ASTM and ISO tests; 5 mm/min.
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil..
Tensile Strength, Ultimate 170 MPa
24700 psi
5 mm/min; ISO 527-2/1A
Global GP-5180-30 PET 30% Glass Reinforced PET Polyester  (discontinued **)
Information provided by Global Polymers Corporation.
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol..
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM D638
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf..
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM data at 5 mm/min.
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
Tensile Strength, Ultimate >= 170 MPa
>= 24700 psi
MetalTek MTEK 76-6-18 HI LEAD Cast UNS C94100 Bearing Bronze
Popular alloy with score resistance, structural uniformity, shear properties, compressive strength and low cost.Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic partsInform..
Tensile Strength, Ultimate >= 170 MPa
>= 24700 psi
MetalTek MTEK 79-6-15 HI LEAD Cast UNS C93900 Bearing Bronze
Popular alloy with score resistance, structural uniformity, shear properties, compressive strength and low cost.Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic partsInform..
Tensile Strength, Ultimate 170 MPa
24700 psi
ICE Al2O3 94
Data provided by the manufacturer, International Ceramic Engineering.
Tensile Strength, Ultimate 170 MPa
24700 psi
ICE Al2O3 96
Data provided by the manufacturer, International Ceramic Engineering.
Tensile Strength, Ultimate 170 MPa
24700 psi
ICE Al2O3 99.5
Data provided by the manufacturer, International Ceramic Engineering.
Tensile Strength, Ultimate 170 - 340 MPa
24700 - 49300 psi
Materion Brush 1915â„¢ Annealed Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Ultimate 170 MPa

@Temperature 980 °C
24700 psi

@Temperature 1800 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Tensile Strength, Ultimate 170 MPa
24700 psi
Sapco 95% Aluminum Oxide
Information provided by Sapco.
Tensile Strength, Ultimate 170 MPa
24700 psi
ISO 527
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Tensile Strength, Ultimate 170 MPa
24700 psi
ASMT D638
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Novamid® 1010GH30 NAT PA6-GF30
30% Glass Reinforced, Heat Stabilized, Injection Molding
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Novamid® 1013G30 1 NA PA6-GF30
30% Glass Reinforced, Injection Molding
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30
30% Glass Reinforced, Heat Stabilized, Injection Molding
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Novamid® 3021GH30 NAT PA66-GF30
30% Glass Reinforced, Heat Stabilized
Tensile Strength, Ultimate 170 MPa
24700 psi
cond; ISO 527-1/-2
DSM Stanyl® 46HF4550 PA46-GF50
50% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications
Tensile Strength, Ultimate 170 MPa
24700 psi
dry; ISO 527-1/-2
DSM Stanyl® 46SF5030 PA46-GF30 FR(17)
30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow
Tensile Strength, Ultimate 170 MPa
24700 psi
5mm/min; ISO 527
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d..
Tensile Strength, Ultimate 170 MPa
24700 psi
5mm/min; ISO 527
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry)
Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi..
Tensile Strength, Ultimate 170 MPa
24700 psi
5mm/min; ISO 527
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..
Tensile Strength, Ultimate 170 MPa
24700 psi
Same value from ASTM and ISO tests; 5 mm/min.
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava..
Tensile Strength, Ultimate 170 MPa

@Thickness 5.00 mm,
Temperature 200 °C
24700 psi

@Thickness 0.197 in,
Temperature 392 °F
Typical L-T Direction
Aleris HOGAL 5558 Aluminum 5026 H14/H34
HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris.
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM D638
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy  (discontinued **)
Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo..
Tensile Strength, Ultimate 170 MPa
24700 psi
5mm/min; ISO 527
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Copyright © lookpolymers.com All Rights Reserved