| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 2.84 MPa | 412 psi | ASTM D638 |
|
Proto3000 CastForm™ PS Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short bur..
|
|||
| Tensile Strength, Ultimate | 2.84 MPa | 412 psi | JIS K6301 |
|
Stellarchem LP-870 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Tensile Strength, Ultimate | 2.84 MPa | 412 psi | Infiltrated; ASTM D638 |
|
ALM PS 200 Prototyping Polymer
Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor..
|
|||
| Tensile Strength, Ultimate | 2.84 MPa | 412 psi | ASTM D638 |
|
3D Systems CastForm™ PS Plastic for SLS® Systems
For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo..
|
|||