| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638-61T |
|
Rotuba 860S Ethyl Cellulose
Data provided by the manufacturer.
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638 |
|
NCMT NanoPAC™ S203 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ISO 527 |
|
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ISO 527 |
|
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM Data |
|
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene
(discontinued **)
STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins...
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | DIN 53455 |
|
Ineos Nova S-4200 Medium Impact Compact Polystyrene
(discontinued **)
Medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | DIN 53455 |
|
Ineos Nova S-7600MG Compact Polystyrene Microgranulates
(discontinued **)
High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, ..
|
|||
| Tensile Strength, Ultimate |
28.0
-
46.0
MPa @Temperature 60.0 - 90.0 °C |
4060
-
6670
psi @Temperature 140 - 194 °F |
Average value: 37.0 MPa Grade Count:1 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638 |
|
NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin
(discontinued **)
Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided..
|
|||
| Tensile Strength, Ultimate |
28.0
MPa @Thickness 1.60 mm |
4060
psi @Thickness 0.0630 in |
Sintered moldings; ASTM D4894/4895 |
|
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder
(discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder ..
|
|||
| Tensile Strength, Ultimate |
28.0
-
116
MPa @Temperature -40.0 - 80.0 °C |
4060
-
16800
psi @Temperature -40.0 - 176 °F |
Average value: 73.0 MPa Grade Count:2 |
|
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | |
|
Kuraray HYBRAR® PH8 Polypropylene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | at max load; ISO 527 |
|
A. Schulman FORMION™ FI 397 Ionomer
Information provided by A. Schulman.
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | at max load; ISO 527 |
|
A. Schulman FORMION™ FI 397 Ionomer
Information provided by A. Schulman.
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | DIN 53504 |
|
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | at max load; ISO 527 |
|
A. Schulman FORMION™ FI 397 Ionomer
Information provided by A. Schulman.
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638/D412 |
|
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System
0.1 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offi..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638/D412 |
|
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..
|
|||
| Tensile Strength, Ultimate | >= 28.0 MPa | >= 4060 psi | DIN 53 504 |
|
Dow BETAMATE™ 7000/7050 L Epoxy
Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | |
|
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638/D412 |
|
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | Dynamic tensile strength |
|
Channel Industries 5500 Lead Zirconate Titanate Piezoelectric
Navy Type IICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | Dynamic tensile strength |
|
Channel Industries 5700 Lead Zirconate Titanate Piezoelectric
Navy Type VICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D638 |
|
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Tensile Strength, Ultimate | 28.0 MPa | 4060 psi | ASTM D412-80 |
|
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)&
Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Reinforcing fillers not needed..
|
|||