Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 250 MPa
>= 36300 psi
MetalTek NAVY G 1% LEAD Cast UNS C92300 Bearing Bronze
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C92300; Cast Grade C92..
Tensile Strength, Ultimate 250 - 330 MPa
36300 - 47900 psi
SSAB Tunnplat Docol® 4D Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 250 MPa
36300 psi
Sapco 98% Aluminum Oxide
Information provided by Sapco.
Tensile Strength, Ultimate 250 MPa
36300 psi
Fiber value estimated from tenacity; ASTM D3218
Total PPH 3762 Polypropylene, Extrusion Grade
Homopolymer fiber grade for staple fiber and multifilament yarnsFading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.Process ..
Tensile Strength, Ultimate 250 MPa
36300 psi
dry; ISO 527-1/-2
DSM Stanyl® 46HF4550 PA46-GF50
50% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications
Tensile Strength, Ultimate 250 MPa
36300 psi
China Tungsten STG60-25 PM Structural Parts
Information provided by China Tungsten
Tensile Strength, Ultimate 250 MPa
36300 psi
China Tungsten STG90-25 PM Structural Parts
Information provided by China Tungsten
Tensile Strength, Ultimate 250 MPa
36300 psi
Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.2 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Tensile Strength, Ultimate 250 - 310 MPa
36300 - 45000 psi
ArcelorMittal 07 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC07) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au..
Tensile Strength, Ultimate 250 MPa

@Thickness 5.00 - 12.0 mm
36300 psi

@Thickness 0.197 - 0.472 in
Typical L-T Direction
Aleris HOGAL 5558 Aluminum 5026-O/H111
HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris.
Tensile Strength, Ultimate 250 MPa
36300 psi
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Tensile Strength, Ultimate >= 250 MPa
>= 36300 psi
Guaranteed Minimum L-T Direction
Aleris HOGAL 5558 Aluminum 5026 H14/H34
HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris.
Tensile Strength, Ultimate 250 MPa
36300 psi
dry; ISO 527-1/-2
DSM Stanyl® TS200F10 PA46-GF50