Polymer Property : Tensile Strength, Ultimate = 398 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.75 MPa
398 psi
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Tensile Strength, Ultimate 2.75 MPa
398 psi
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Tensile Strength, Ultimate 2.75 MPa
398 psi
Momentive Performance Materials RTV108 One Component Acetoxy Adhesive Sealant, Translucent
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Tensile Strength, Ultimate 2.75 MPa
398 psi
Momentive Performance Materials RTV109 One Component Acetoxy Adhesive Sealant, Aluminum
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..