Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 4.51 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.51 MPa
654 psi
Momentive Performance Materials RTV133 Black Adhesive Sealant, Flame Retardant Paste
One-part alkoxy cure. Typical uses: As a sealant on firewalls or as a flame retardant coating. Use in switching devices, motors, and high voltage transformers.Data provided by the manufacturer, GE..
Tensile Strength, Ultimate 4.51 MPa
654 psi
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant
RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re..
Tensile Strength, Ultimate 4.51 MPa
654 psi
JIS K6301
Stellarchem MP-930HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..