| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638-95 |
|
Multibase Multi-Flex® TPO D-6500
Multi-Flex® D 6500 is well suited for TPO extrusion applications and certain high value molded parts for the telecommunications industry.Data provided by Multibase.
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
NCMT NanoPAC™ HG500 High Performance Polypropylene Nanocomposite
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
|
|||
| Tensile Strength, Ultimate | 29.0 - 147 MPa | 4210 - 21300 psi | Average value: 70.3 MPa Grade Count:77 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Rotuba MS Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
|
|||
| Tensile Strength, Ultimate | 29.0 - 51.0 MPa | 4210 - 7400 psi | Average value: 39.7 MPa Grade Count:14 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
|
|||
| Tensile Strength, Ultimate |
29.0
MPa <br>@Temperature 90.0 °C
|
4210
psi <br>@Temperature 194 °F
|
ISO 527 |
|
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
|
|||
| Tensile Strength, Ultimate |
29.0
MPa <br>@Temperature 60.0 °C
|
4210
psi <br>@Temperature 140 °F
|
ISO 527 |
|
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
|
|||
| Tensile Strength, Ultimate | 29.0 - 138 MPa | 4210 - 20000 psi | Average value: 72.7 MPa Grade Count:55 |
|
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
|
|||
| Tensile Strength, Ultimate | 29.0 - 40.0 MPa | 4210 - 5800 psi | Average value: 34.4 MPa Grade Count:16 |
|
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **)
Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | Vulcanized |
|
KKPC KOSYN 1500NF Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
LyondellBasell Astryn 65F4-2 Polypropylene Homopolymer, 20% Talc
Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, excellent impact and stiffness balance, good dimensional stability, excellent heat resistance, good colo..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM Data |
|
Styron Magnumâ„¢ 9043 ABS, High Gloss Sheet Extrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Elastomer Engineering Elastamide 300 Elastomer Modified RIM Nylon 6
22% crystallinity. Information supplied by Elastomer Engineering.
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ISO 37 |
|
Lubrizol ESTANE® 58280 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Eastman PROVISTA Copolymer PETG Copolyester
Color, b* CIELAB, Illuminant D6500, 10° Observer is 0.61 per ASTM D 2244.Product Description: PROVISTA Copolymer is a resin specifically developed for extrusion into profiles where aesthetics like..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638/D412 |
|
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ISO 527 |
|
DSM Fibre Intermediates Nyrim® 3000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | Die C (35 min / 145°C); ASTM D412 |
|
Dow Buna® SB 1502 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Buna® SB 1502 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. A non-discoloring stabilizer is added during the production process. Buna® SB 1502 - Sc..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM Data |
|
Dow Retain® PS-4578 Polystyrene
Data provided by Dow Chemical.
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | |
|
3M Jet-Weld™ TE-100 Adhesive
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Extrudable grade with medium set time and low viscosity ideal for bonding wood. Ca..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Buckeye Polymers BP RPP 3019 TU Polypropylene, 30% Mineral Filled
UV StabilizedThis Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistan..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
|
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
|
|||
| Tensile Strength, Ultimate |
29.0
-
80.0
MPa <br>@Temperature -40.0 - 120 °C
|
4210
-
11600
psi <br>@Temperature -40.0 - 248 °F
|
Average value: 45.0 MPa Grade Count:4 |
|
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM Data |
|
Americas Styrenics Styron® 425 High Impact Polystyrene
(discontinued **)
STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper..
|
|||
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ISO 37 |
|
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade)
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible..
|
|||
| Tensile Strength, Ultimate | 29.0 - 39.0 MPa | 4210 - 5660 psi | ISO 527 |
|
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
|
|||
| Tensile Strength, Ultimate | 29.0 - 153 MPa | 4210 - 22200 psi | Average value: 101 MPa Grade Count:42 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
|
|||