Polymer Property : Tensile Strength, Ultimate = 455 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.14 MPa
455 psi
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
One-part acetoxy cure. Typical uses: Heavy bodied adhesive sealant for formed-in-place gasketing. Good oil resistance.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
Tensile Strength, Ultimate 3.14 MPa
455 psi
JIS K6301
Stellarchem 475-860N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Tensile Strength, Ultimate 3.14 MPa
455 psi
500 mm/min; ASTM D 412
Zylog Neoplast® 145 FT EB Thermoplastic Vulcanizate
Neoplast 145 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, ..