Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 5000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite
Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
MF-5062 Polyurethane-based Biomedical Elastomer
Tensile Strength, Ultimate 34.5 MPa
5000 psi
TM R050-36
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Tensile Strength, Ultimate 34.5 - 90.0 MPa
5000 - 13100 psi
Average value: 52.7 MPa Grade Count:35
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Ultimate 34.5 - 44.8 MPa
5000 - 6500 psi
Average value: 39.5 MPa Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 34.5 - 180 MPa
5000 - 26100 psi
Average value: 93.7 MPa Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM Data
Styron Magnumâ„¢ 344CC ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM Data
Styron Magnumâ„¢ 9095 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM Data
Styron Magnumâ„¢ 9450P ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM Data
Styron Magnumâ„¢ 9700HF ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Williams Advanced Alloys WS225 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Williams Advanced Alloys WS257 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D638
Ecomass® 1080ZB92 Filled Polyamide
Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester
BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..
Tensile Strength, Ultimate 34.5 - 41.4 MPa
5000 - 6000 psi
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester
BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a..
Tensile Strength, Ultimate 34.5 - 62.1 MPa
5000 - 9000 psi
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati..
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium ..
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester
BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium..
Tensile Strength, Ultimate 34.5 - 68.9 MPa
5000 - 10000 psi
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
MF-5040 Polyurethane-based Biomedical Elastomer
Tensile Strength, Ultimate 34.5 MPa
5000 psi
TM R050-36
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive
Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili..
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
MF-5056 Polyurethane-based Biomedical Elastomer