Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 540 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 540 MPa

@Temperature 250 °C
78300 psi

@Temperature 482 °F
EN min.; EN 10002-5
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Tensile Strength, Ultimate 540 MPa

@Temperature 100 °C
78300 psi

@Temperature 212 °F
EN min.; EN 10002-5
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 540 MPa
78300 psi
Typical after Solution Annealing
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel
Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b..
Tensile Strength, Ultimate 540 MPa
78300 psi
Typical after Solution Annealing
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r..
Tensile Strength, Ultimate 540 MPa

@Temperature 550 °C
78300 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 2010°F (1100°C). It contains rare-earth additions for increased oxidation resistance, especially und..
Tensile Strength, Ultimate 540 MPa

@Temperature 550 °C
78300 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nicke..
Tensile Strength, Ultimate 540 MPa
78300 psi
Annealed
Special Metals NILOMAG® Alloy 77
A nickel-iron alloy with additions of copper and molybdenum. It is a low-loss, soft-magnetic alloy with a high initial permeability. Initial permeability 60,000; maximum permeability 300,000; satu..
Tensile Strength, Ultimate 540 - 640 MPa
78300 - 92800 psi
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Ultimate 540 - 580 MPa
78300 - 84100 psi
T direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 540 - 580 MPa
78300 - 84100 psi
T direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 540 - 580 MPa
78300 - 84100 psi
T direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 540 - 580 MPa
78300 - 84100 psi
T direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 540 - 610 MPa
78300 - 88500 psi
ArcelorMittal FB 540 Hot rolled ferrite-bainite steel
Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steel..
Tensile Strength, Ultimate 540 MPa

@Temperature 200 °C
78300 psi

@Temperature 392 °F
EN min.; EN 10002-5
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 540 MPa

@Temperature 250 °C
78300 psi

@Temperature 482 °F
EN min.; EN 10002-5
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 540 MPa

@Temperature 550 °C
78300 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals INCOLOY® Alloy 020
A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellen..