Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.0 - 117 MPa
8270 - 16900 psi
Average value: 71.1 MPa Grade Count:13
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Tensile Strength, Ultimate 57.0 - 130 MPa
8270 - 18900 psi
Average value: 104 MPa Grade Count:23
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7100-15 Polycarbonate
CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7101-15 Polycarbonate
CALIBREâ„¢ 7101-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7102-15 Polycarbonate
CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7103-15 Polycarbonate
CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 2000 Phenolic, Granular, Injection Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 2308 Phenolic, Granular, Injection Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 2369 Phenolic, Granular, Transfer Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 3303 Phenolic, Granular, Injection Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 7021 Phenolic, Granular, Injection Molded
PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compressio..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ISO 527-1, 2
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Low friction, Low wear
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 6301 Phenolic, Granular, Injection Molded
PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ISO 527-1, 2
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ISO 527-1/-2
DSM Arnite® TM4 440 (PBT+PET)-MD20
20% Mineral Reinforced
Tensile Strength, Ultimate 57.0 MPa
8270 psi
BASF Polystyrol® 168 NO Polystyrene (Europe)
High molecular, heat-resistant grades for the extrusion of low-taint food packaging, especially BOPS.Data was collected by ISO methods and provided by BASF.
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ATSM D638
Ashley Polymers Ashlene® 525 Nylon 66
High impact Nylon 66 with good stiffness for injection molding.Data provided by the manufacturer
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
A. Schulman ComAlloy Comtuf® 106 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled, Impact Modified, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has ..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Chem Polymer Chemlon 280 Nylon 6, High Impact
A highly impact modified nylon 6 exhibiting excellent toughness and flexibility.Data provided by the manufacturer, Chem Polymer.
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Plenco 7552 Phenolic, Nodular, Transfer Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Tensile Strength, Ultimate 57.0 - 145 MPa
8270 - 21000 psi
Average value: 104 MPa Grade Count:24
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ATSM D638
Ashley Polymers Ashlene® R190H Acetal
General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3..