Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 58.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638-95
Multibase Multi-Pro® 2005 RC I High Impact 20% Glass Polypropylene
Multi-Pro 2005 RC I is a chemically coupled polypropylene compound with increased stiffness, flex strength and excellent impact resistance. This product is geared for top engineering plastics appli..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Nylene® CX3451 Translucent Nylon Copolymer
Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Nylene® Naxel™ PC10 Polycarbonate
Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources C..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
TM R050-36
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D412
2065D Polyurethane-based Biomedical Elastomer
Tensile Strength, Ultimate 58.6 - 72.4 MPa
8500 - 10500 psi
Average value: 64.5 MPa Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedNaturalPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 58.6 - 92.2 MPa
8500 - 13400 psi
Average value: 80.9 MPa Grade Count:7
Overview of materials for Thermoplastic Polyimide, Unfilled
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled
Conductive Carbon, Powder Modified
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM Data
Styron CALIBREâ„¢ 891 10 Polycarbonate, General Purpose
CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM Data
Styron CALIBREâ„¢ 891 20 Polycarbonate, General Purpose
CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Styron EMERGEâ„¢ 4800-10 Polycarbonate
EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Styron EMERGEâ„¢ 4850-10 Polycarbonate
EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Styron EMERGEâ„¢ 4850-19 Polycarbonate
EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 893-10 Polycarbonate
CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 893-20 Polycarbonate
CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Styron EMERGEâ„¢ 4800-19 Polycarbonate
EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
after optimum cure
Armstrong C-7/H20 Epoxy Adhesive
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Abatron AboCast 7703-21/AboCure 7703-22 (B) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 58.6 MPa
8500 psi
TM R050-36
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
TM R050-36
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad..
Tensile Strength, Ultimate 58.6 MPa
8500 psi
TM R050-36
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Tensile Strength, Ultimate 58.6 MPa

@Temperature 150 °C
8500 psi

@Temperature 302 °F
ISO 62
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..
Tensile Strength, Ultimate 58.6 - 72.4 MPa
8500 - 10500 psi
ASTM D638
Premix Premi-Glas® 1200-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa..
Copyright © lookpolymers.com All Rights Reserved