| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 8.90 MPa | 1290 psi | ASTM D412 |
|
Multibase Multi-Flex® TPE A 8502-SR BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
|
|||
| Tensile Strength, Ultimate | 8.90 MPa | 1290 psi | ASTM D412 |
|
Multibase Multi-Flex® TPE A 9002-SR BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
|
|||
| Tensile Strength, Ultimate | 8.90 MPa | 1290 psi | TPE-0153 (ASTM D 412) |
|
ExxonMobil Vyram™ 9271-85 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure..
|
|||