Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plaskolite Optix® CA-924 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Good impact strength.
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Good impact strength.
Tensile Strength, Ultimate 58.0 MPa
<br>@Temperature 1095 °C
8410 psi
<br>@Temperature 2003 °F
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Glastic Laminates/Shapes 1580 Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements.
Tensile Strength, Ultimate 58.0 MPa
<br>@Temperature 22.0 °C
8410 psi
<br>@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP
SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is ..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7100-8 Polycarbonate
CALIBREâ„¢ 7100-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7101-8 Polycarbonate
CALIBREâ„¢ 7101-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7102-8 Polycarbonate
CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
50 mm/min; ISO 527-2
Styron CALIBREâ„¢ 7103-8 Polycarbonate
CALIBREâ„¢ 7103-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
0.2 in/min; ASTM D638
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 4327 Phenolic, Granular, Compression Molded
PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electri..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 4527 Phenolic, Granular, Transfer Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 7500 Phenolic, Granular, Compression Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 7507 Phenolic, Granular, Transfer Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ISO 527-1, 2
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ISO 527-1, 2
Polyplastics Duranex® 500FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
5mm/min; ISO 527-1, 2
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics.
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability
10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 2408 Phenolic, Granular, Injection Molded
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
DIN 53504
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
A. Schulman ComAlloy Voloy® 411 Mineral Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ISO 527
Brueggemann Chemical Nyrim® 1000 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D651
Resinoid 2016 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D651
Resinoid 2016P Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Plenco 3557 Phenolic, Granular, Transfer Molded
PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Styrolution NAS® 21 Acrylic Copolymer
Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma..
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ATSM D638
Ashley Polymers Ashlene® R190H2 Acetal
General purpose economy grade copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for maximum weatherability. Available in Natural and Black. Natural: Designated R190..