| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638-95 |
|
Multibase Multi-Pro® 2005 RC I High Impact 20% Glass Polypropylene
Multi-Pro 2005 RC I is a chemically coupled polypropylene compound with increased stiffness, flex strength and excellent impact resistance. This product is geared for top engineering plastics appli..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Nylene® CX3451 Translucent Nylon Copolymer
Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Nylene® Naxel™ PC10 Polycarbonate
Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources C..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | |
|
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D412 |
|
2065D Polyurethane-based Biomedical Elastomer |
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
|
PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedNaturalPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
|
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Tensile Strength, Ultimate | 58.6 - 92.2 MPa | 8500 - 13400 psi | Average value: 80.9 MPa Grade Count:7 |
|
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
| Tensile Strength, Ultimate | 58.6 - 221 MPa | 8500 - 32100 psi | Average value: 116 MPa Grade Count:81 |
|
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
|
|||
| Tensile Strength, Ultimate | 58.6 - 82.7 MPa | 8500 - 12000 psi | Average value: 66.4 MPa Grade Count:4 |
|
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled
Conductive Carbon, Powder Modified
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM Data |
|
Styron CALIBREâ„¢ 891 10 Polycarbonate, General Purpose
CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM Data |
|
Styron CALIBREâ„¢ 891 20 Polycarbonate, General Purpose
CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Styron EMERGEâ„¢ 4800-10 Polycarbonate
EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Styron EMERGEâ„¢ 4850-10 Polycarbonate
EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Styron EMERGEâ„¢ 4850-19 Polycarbonate
EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ 893-10 Polycarbonate
CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | 50 mm/min; ASTM D638 |
|
Styron CALIBREâ„¢ 893-20 Polycarbonate
CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Styron EMERGEâ„¢ 4800-19 Polycarbonate
EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Styron EMERGEâ„¢ 4800-7 Polycarbonate
EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
|
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc.
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | after optimum cure |
|
Armstrong C-7/H20 Epoxy Adhesive
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
|
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
|
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
|
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
|
|||
| Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
|
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..
|
|||
| Tensile Strength, Ultimate |
58.6
MPa @Temperature 150 °C |
8500
psi @Temperature 302 °F |
ISO 62 |
|
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..
|
|||