| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 966 MPa | 140000 psi | |
|
ATI Allvac® 6-6-2 Titanium Alloy, Heat Treatment: 718°C (1325°F) Anneal
Data provided by Allvac.Applications: Airframes, jet engines, rocket engine cases, nuclear reactor components, ordnance components.
|
|||
| Tensile Strength, Ultimate | 966 MPa | 140000 psi | |
|
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal
Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire.
|
|||
| Tensile Strength, Ultimate | 966 MPa | 140000 psi | |
|
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization
Data provided by Allvac.Applications: High performance helicopter transmission gears, components.
|
|||