Polymer Property : Tensile Strength, Ultimate = 9860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.0 - 68.0 MPa
4930 - 9860 psi
Average value: 55.1 MPa Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Tensile Strength, Ultimate 39.0 - 68.0 MPa
5660 - 9860 psi
Average value: 52.0 MPa Grade Count:43
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..