Polymer Property : Shear Strength = 13.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Shear Strength 0.352 - 13.8 MPa
51.0 - 2000 psi
Average value: 3.99 MPa Grade Count:7
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Shear Strength 10.3 - 13.8 MPa
1500 - 2000 psi
ITW Plexus Plexusâ„¢ MA320 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent low temperature and toughness properties.Information provided by Illinois Tool Works.
Shear Strength 10.3 - 13.8 MPa
1500 - 2000 psi
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works.
Shear Strength 11.0 - 13.8 MPa
1600 - 2000 psi
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Shear Strength 10.3 - 13.8 MPa
1500 - 2000 psi
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
Shear Strength 3.45 - 13.8 MPa
500 - 2000 psi
Lap; ASTM D1002
3M Scotch-Weld™ GM18 Gasket Maker Anaerobic Adhesive
3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal..