| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Shear Strength | 10.3 MPa | 1500 psi | Cured 6 minutes at 130°C, Al/Al |
|
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System
Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco..
|
|||
| Shear Strength | >= 10.3 MPa | >= 1500 psi | Cured 10 minutes at 120°C, Al/Al (etched) |
|
Resin Technology Group TIGA 951 One-Part Silver Conductive Epoxy System
Cure 10 minutes at 120°CTIGA 951 is an electrically conductive, silver-filled epoxy adhesive recommended for electronic bonding and sealing applications. This one-part, smooth paste formulation of ..
|
|||
| Shear Strength | 10.3 - 13.8 MPa | 1500 - 2000 psi | |
|
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works.
|
|||
| Shear Strength | 10.3 - 12.4 MPa | 1500 - 1800 psi | |
|
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works.
|
|||
| Shear Strength | 10.3 - 12.4 MPa | 1500 - 1800 psi | |
|
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
|
|||
| Shear Strength | 10.3 - 13.8 MPa | 1500 - 2000 psi | |
|
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
|
|||
| Shear Strength | >= 10.3 MPa | >= 1500 psi | Tensile lap, Al to Al |
|
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or ..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Lap |
|
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a ..
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Overlap, Steel Solvent Wipe; ASTM D1002-72 |
|
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Aluminum Overlap; ASTM D1002 |
|
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Aluminum Overlap; ASTM D1002 |
|
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Fiberglass |
|
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Sanded Aluminum |
|
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Overlap |
|
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, PP, Cohesive Failure |
|
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, EC 3924 Primed Al/HDPE (non-abraded Al), Cohesive Failure |
|
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Phenolic (IPA/abrade/IPA), Substrate Failure; ASTM D1002 |
|
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, CRS-MEK/abrade/MEK-Adhesive/Cohesive Failure; ASTM D1002 |
|
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Steel; ASTM D1002-64 |
|
3M Scotch-Weld™ CA40H Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity version of CA40 and better void filling capabilities.Information provided by 3M
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Sanded Aluminum |
|
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Gel Coat (3/16" thick), Substrate Failure |
|
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, CRS/CRS after 7 days of Immersion in Gasoline |
|
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
|
|||
| Shear Strength |
10.3
MPa @Temperature 81.0 - 83.0 °C |
1500
psi @Temperature 178 - 181 °F |
Stored 1 year, 22-26°C, Minimum MIL-A-8623 Type III Requirement |
|
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Aluminum Overlap; ASTM D1002 |
|
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar..
|
|||
| Shear Strength |
10.3
MPa @Temperature -55.0 °C |
1500
psi @Temperature -67.0 °F |
Aluminum Overlap; ASTM D1002 |
|
3M Scotch-Weld™ DP 3501 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Stainless Steel/Stainless Steel |
|
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Copper/Copper |
|
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Brass/Brash |
|
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | Overlap, Cold Rolled Steel |
|
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..
|
|||
| Shear Strength | 10.3 MPa | 1500 psi | cured, grit-blasted steel; ASTM D1002 |
|
3M Scotch-Weld™ RT300B Rubber-Toughened Instant Adhesive
3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon..
|
|||